View previous topic :: View next topic |
Author |
Message |
rsdean
Joined: 27 Jun 2002 Posts: 52 Location: NE Maryland
|
Posted: Sat Nov 01, 2003 12:04 pm Post subject: |
|
|
I noticed that the back of my Pacemaker is starting to show signs of corrosion, on the left side of the ground glass holder. (Spring back.) Is there any easy* way of arresting this and repainting the affected parts? I probably can't manage the black crackle paint...
Rob Dean
*Laborious would be OK, too, as long as fairly straightforward.
|
|
Back to top |
|
 |
RichS
Joined: 18 Oct 2001 Posts: 1468 Location: South of Rochester, NY
|
Posted: Sat Nov 01, 2003 5:11 pm Post subject: |
|
|
I've had quite a few pieces with the corrosion. I can't say for long term, but I usually give it a good brushing with a brass brush to remove as much as I can and then paint it. I haven't worried about the crackle finish yet. That can easily be done if you don't mind repainting a large area as it works best sprayed. So I use an automotive touch-up paint that comes in small jars at the auto store. It's worked great so far, but I have no idea if it's really preventing any further corrosion? Maybe Rustoleum would be better?
_________________ ----------------------------------------
"Ya just can't have too many GVIIs"
---------------------------------------- |
|
Back to top |
|
 |
disemjg
Joined: 10 Jan 2002 Posts: 474 Location: Washington, DC
|
Posted: Sat Nov 01, 2003 11:37 pm Post subject: |
|
|
If the corrosion is extensive, be sure to remove the back from the camera body as there is probably corrosion umder it, and it needs to be fixed. The brass brush mentioned in the earlier reply is good to clean off spots that have corrosion. I use Krylon semi-matte spray on large pieces, or brushing lacquer on small spots. |
|
Back to top |
|
 |
45PSS
Joined: 28 Sep 2001 Posts: 4081 Location: Mid Peninsula, Ca.
|
Posted: Sun Nov 02, 2003 5:41 am Post subject: |
|
|
A brass or stainless steel brush on a variable speed Dremel works great. The advantage is less elbow grease and if the corrosion is spreading under the paint its easier to get at, paint in non corroded areas will not come off as easily.
Charles
_________________ The best camera ever made is the one that YOU enjoy using and produces the image quality that satifies YOU. |
|
Back to top |
|
 |
bertsaunders
Joined: 20 May 2001 Posts: 577 Location: Bakersfield California
|
Posted: Mon Nov 03, 2003 8:32 pm Post subject: |
|
|
Aluminum and steel are not compatables, so in many cases, a white looking powder appears on the aluminum parts....steel screws often freeze solid in tapped holes! WD40 will remove the powder, and in most cases, free the screws, you will still in most cases have to do follow with brushes or cloth....it also will remove glue residue from masking tapes and stick on labels.....as always, dont use it to drowned the item, cause a "little bit will do-ya!" Bert |
|
Back to top |
|
 |
troublemaker
Joined: 24 Nov 2003 Posts: 715 Location: So Cal
|
Posted: Tue Dec 02, 2003 8:25 am Post subject: |
|
|
I have been working on aluminum sialboat rigs for years, and the big problme is dissimilar metals as mentioned above. for those who plan to keep and preserve for longevity, there are various products one can apply to fasteners that help prevent corrosive bonding that ofetn ends in broken screw heads and lot sof cussing. The cheapest and least preventative way to go is a littel heavy grease. We also use lanolin paste, which is widely available and comes in a handy little tub at places like marine stores. There is a product called alumilastic that i like but have not been able to find lately. It looks a littel like a never sieze but is more like calking paste. The best product i currently know of and use on all our high end projects is something called tef-gel. it is sticky, gooey, and goes a long way, and is about as tenacious as anything i have ever got my fingers in. However, the stuff is expensive, and unless you have a boat, or a lot of cameras, be prepared to pay a hundred bucks for a tub!
I wouldn't recomend any kind of anti-seize product because they are all metal based, everything form graphite, old led-plate products, copper and or nickle etc...these may promote rather than hinder corrosion, thus the teflon based gels are supperb.
that's my two sense worth.
good luck gettign paint to stick after all that son-of-a-gun and lemon pledge, try a little acetone or MEK before applying paint.
steve
_________________ Anyone can buy tools... |
|
Back to top |
|
 |
ariel
Joined: 03 Dec 2003 Posts: 7 Location: lynchburg, va
|
Posted: Fri Dec 05, 2003 6:38 pm Post subject: |
|
|
a friend suggested naval jelly when i encountered the same problem.
i haven't tried it, but i did use some WD40 after brushing and sanding a little.
the corrosion has not come back since.
 |
|
Back to top |
|
 |
|